Nickel in White Gold

How can the average person tell if there is nickel in white gold?

It is sometimes slightly magnetic, but not always

There are test kits like this one that are readily available. They will
not work if the item is recently rhodium plated though.

Esta Jo Schifter, this would be a definitive
for you to test your ring.