Neycraft Furnace Question

Thanks Craig. I do see the thermocouple for the oven as you stated. I was looking to add a second thermocouple from my Paragon oven controller. With my old oven the heating elements where exposed so I was able to drill a hole through the case and fire brick in the back of oven. My fix there was to suspend Paragon thermocouple in top vent hole about 3’’ inside oven chamber. I just did a burn out and both pyrometers temp paired exactly and my 1300 cone was well fired.

I am wondering what repairs you had to do to your oven?

Cheers
Franz