Michael Mathews - Rings

The X-ring is approximately 3 carat total weight. I carved a wax
and cast the 14K white gold X and soldered on seven independent 14K
yellow gold twisted wire shank. This was a custom design for a
customer. The white gold ring is also a custom for a customer. I
carved the wax and set the stones.