Hey Lars… For the very reason of nickel alergys, we cast in 18k
Paladium white gold, mostly for our retail customers. No alergy
problems…and if you ever tried to set stones in white gold you
won’t believe the difference. Easier than 18k yellow! e-mail if
you want to know more