Back to Ganoksin | FAQ | Contact

Motorizing a Durston rolling mill?


#1

Hello Donna,

I attached a large diameter pulley wheel in place of the handle, and
use a belt driven from an old motor. It meets my needs, and speeds up
the rolling process.

Your husband can probably do better, and use gears. I’ll send you
pictures as soon as I can take them.

Regards,
Larry