Thanks Jeff,
I have a suggestion worth trying on making a metal mold. It is a product sold by Cotronics..... called Duralco 4540.
I’ll look it up and evaluate it. I’m real close on the method and a
couple of experiments have turned out well. I’m just waiting to get
to a point where I can replicate it, document it, picture it, and
share it.
And, it sounds like the process would be very similar but substitute
the epoxy for the pewter. And if I can do it with the pewter, it
would be more economical, I buy scrap pewter plates and mugs for
under $3 a pound.
Thanks for your thoughts and keeping this thread alive.
Regards
RLW (Ronald L. Wade)