IJS makes Money Clip bodies in sterling, Nickel “silver”, and red
brass. They are sweated on to a face plate, or even engraved
directly. They are just metal strips just folded over.

John, you are accurate in saying that there’s a capacity threshold
with the money clip. We at IJS like to think that’s a loss reducer in
the unfortunate event of a mugging.

I can be hailed off-list for money clips, tie clips, and so much
more. We do have a “gator-jaw” tie clip, as well as a “slice of a
money clip” tie bar. Just not many cloth-tie wearers. It’s more of a
bola-tie crowd we service.