Hi all, I need to find a magnetic clasp in Sterling Silver for a
client with disabilities.  I know I have seen them somewhere but
can't find it in my catalogs.  Can anyone help me? 

Dear Deb, The Bead Box sells them as well as Metalliferous. They are
not in the Metallierous catalog you have to ask for them.

Cathy Wheless
www.cathywheless.com