Hello
I must’ve been lost the phone number of jewelry casting company. I
am pretty new in chicago and I don’t know much about this area. I got
the number from one of members in ganoksin and I lost it. 
Could you anyone tell me the casting company’s name and phone number
around chicago area? I make jewelry for individuals so I don’t make
a lot of jewelry at once.
Thank you.
Shin
Hi Shin,
Casting House is located in the 5 South Wabash jewelry building
downtown, as are most of the Chicago casters. If you refresh any
Ganoksin page with the square advertisements on the right, our ad
will show up after one or two tries. It is linked to the website.
We occupy the east side of the sixth floor if you would like to visit
us. You also can call the toll free number: 1-877- 927-CAST (2278).
It’s fine that you don’t have big orders- our minimum is one piece.
I hope you enjoy getting to know our great city.
Sincerely,
Jason
Casting House
Hey Shin,
Here are some more Chicago casters and one in MI that is good. Some
casters are better than others depending on what you are trying to
do. You may call me for recommendations. 630.222.6771, or contact me
off list.
A&A Jewelry & Casting
5 S. Wabash, Ste. #417
Kirk - 312.739.0737
Finest Casting
29 E. Madison, 12th floor
Mike - 312.750.1110
Casting House (Formerly G&M Casting?)
312.419.8911
AU Enterprises
Berkley, MI
800.637.2278
Ivan Sagel
www.wyzensageldesigns.com
Casting House (Formerly G&M Casting?) 312.419.8911
If memory serves, the Casting House and Master Casting combined a
few years ago.
What Casting House was before it was Casting House, I don’t recall.
Elaine
http://www.CreativeTextureTools.com
If memory serves, the Casting House and Master Casting combined a
few years ago. What Casting House was before it was Casting House,
I don't recall.
Close. GM Casting (my company) was founded in 1987 and merged with
Casting House (est.1999) in June 2003. Master Casting simply went out
of business when their caster, David Bull, left and co founded
Casting House. David has not been involved in manufacturing since the
merger of our companies, but still works in the industry and is very
well. I am Casting House’s CEO and spend most of my time on r&d and
new product development. Have we met?