Back to Ganoksin | FAQ | Contact

Kunzite the night stone?

Does Kunzite loose its color when worn in sunlight over a 2/3 year
period … and that’s why its called the night stone???

Mark

Kunzite fades in sunlight. That’s how it got it’s reputation as a
night stone.

    Does Kunzite loose its color when worn in sunlight over a 2/3
year period ... and that's why its called the night stone??? 

I don’t know why it’s called the night stone, but it will definitely
fade – and it could be a lot faster than eight months. Keep kunzite
out of bright light (including showcase lighting).

Beth