18K gold
Cloisonne enamel
28mm x 30mm

Pendant

18K gold
Cloisonne enamel
36mm x 32mm

Pendant

28K gold, 24K gold
Cloisonne enamel
38mm x 38mm

Pendant

18K gold, 24K gold
Cloisonne enamel
38mm x 38mm

Pendant

18K gold, 24K gold
Cloisonne enamel
38mm x 38mm

Ring

silver, 24K gold
Cloisonne enamel

Brooch

18K gold, 24K gold
Cloisonne enamel
65mm x 100mm

Pendant

18K gold, 24K gold
Cloisonne enamel
45mm x 52mm

Pendant

24K gold
Cloisonne enamel
35mm x 65mm

Brooch

18K gold, 24K gold
Cloisonne enamel
80mm x 27mm

Pendant

18K gold, 24K gold
Cloisonne enamel
38mm x 38mm

Bracelet

18K gold, 24K gold, silver
Cloisonne enamel
40mm x 40mm

Bracelet

18K gold, 24K gold, silver
Cloisonne enamel
20mm x 20mm

Pendant

24K gold, silver
Cloisonne enamel
60mm x 40mm

Earrings

18K gold, 24K gold
Cloisonne enamel
40mm x 13mm

Earrings

18K gold, 24K gold
Cloisonne enamel
42mm x 26mm

Rings

18K gold, 24K gold
Cloisonne enamel
15mm x 30mm

Rings

18K gold, 24K gold
Cloisonne enamel

Rings

silver
Cloisonne enamel

Rings

18K gold
Cloisonne enamel