Hello Peter, Here a list

Old number system - FEPA grain system - grain size in uM =
Micrometer (1/1000 mm)

2 - 150  - 90  uM
1G - 180 -75  uM
1C - 240 - 60 uM
1F - 500 -30 uM
0  - 600 - 25 uM
2/0 - 1000 - 20 uM
3/0 - 1200 - 15 uM
4/0 - 1500 - 13 uM
6/0 - 2000 - 10 uM
8/0 - 2500 - 8 uM