Anybody know of book/video instruction on mold modifying to make waxes
inject properly(ie debugging mold for injection)

I had problems at first… if you are not supporting the sides of the mold
then buy or make small aluminum (or what ever metal you prefer) supports
and try injecting with the mold in between them… for a starter…

Jim

Earl,
Try Revere academy, I know that they have mold making classes and I think
that they might have a video too. Good luck! Amber

I had problems at first… if you are not supporting the sides of the
mold then buy or make small aluminum (or what ever metal you prefer)
supports and try injecting with the mold in between them… for a

I use pieces of 1/4 inch thick plywood as mold holders and they seem to
work very well