If you're still using Tarn-X, read this!

An e-mail that came to me today:

"I wish I had read your comments on this stuff before I ruined my
expensive Pandora Charms! What in the world can be done to reverse
the damage? I was dipping, rinsing, drying and right before my eyes
they started turning white and chalky. Some of them have black spots
too. I am so sad over this as these charms are many years of
collecting. Please help me if you can. Also I don’t know how to
dispose of this stuff, I don’t want to take chance of some poor
animal coming in contact with it.

Please contact me ASAP if you can be of any help."

Get more on this finish killer here:

http://www.ganoksin.com/gnkurl/ep80r6

Jeff Herman
Hermansilver.com