Back to Ganoksin | FAQ | Contact

Hypoallergenic Gold Earring Findings

Does anyone know of a source for hypoallergenic (non-nickel alloyed)
white and yellow 14kt earring findings, primarily wires and posts?
Several of my customers are having problems with their pierced ears
becoming sore/inflamed with nickel-bearing gold that pass through
the holes. I know they’re out there since companies like Whispers
carry prefabricated earrings using them but have been unable to
locate anyone carrying just the findings. As always, all help
greatly appreciated!

Susan
C Gems

You might try cooksongold.com.

I believe it is illegal to use nickel in gold alloys in the UK, and
they have a wide range.

Usual disclaimer.

Pat

Cookson Precious Metals

Help others make informed buying decisions with Cookson Precious
Metals. We welcome your opinions and experiences with their products,
ordering, customer service and and over all satisfaction.

Write an Anonymous Review
http://www.ganoksin.com/resources/review.php?id=1175

Does anyone know of a source for hypoallergenic (non-nickel
alloyed) white and yellow 14kt earring findings, primarily wires
and posts? 

Yes, at Hoover & Strong our yellow is all nickel free and we offer
the following white in nickel free:

We offer three posts in 14K Palladium.
EP1 .027 X .375
EP2 .030 X .375
EPF12 Fusion tip .027 X .375 partially threaded at 66 threads per
inch.

All are karat stamped and trademarked.

Eugene C. Gentile (Gino)
National Accounts Manager