Back to Ganoksin | FAQ | Contact

How to glue glass on metal?


#1

Is Epoxy 220 or 330 by Hughes Assocs. a workable solution to
gluing gems/glass to metal findings?

Epoxy 220 is amber clear, sets in one hour. Epoxy 330 is water
clear, faster setting.

Dan Woodard


#2

I have not been successful using 330 to bond sterling silver and
obsidian. Larry White