Can one just use a regular old kiln youd use to burnout wax with to do fusing and granulation? And what would the temperature be? Any suggestions on a good online class to learn the two? so far i see victoria lansford online and she doesnt use glue then i see a school in Nyc jewelers academy who teaches in person!
I’m sorry Melissa! I don’t have much advice for online granulation classes.
Kent Raible is an amazing jewelry artist and teacher who specializes in granulation and fused gold. He offers a number of online jewelry classes, but it looks like his granulation classes are in-person. That said, I took a granulation class with Kent many years ago and it was excellent.
Here’s info: https://www.kentraiblestudios.com/granulation-workshops
I don’t know if you used the Orchid forum search function, but there are over a hundred threads on granulation going back for the past decades.
https://orchid.ganoksin.com/search?q=granulation
I hope that helps!!
Jeff
1 Like