Grainy castings troubleshooting

I am Getting grainy castings that break, what am I doing wrong

I am Getting grainy castings that break, what am I doing wrong 

More
Investment casting, melting method etc.

Regards Charles A.

My guess is that your metal is too hot and/or your flask is too hot.
Be a kool jool.

Phillip