Does any of you have experience with gold filled chains by a company called “Garlan Chain Co.”?

I have purchased some samples from them, and so far, I am happy with the quality and their service. However, from my experience, you cannot really tell the true quality of gold filled until you/your customers wear them for months under different conditions.

If you have used this company, have you ever had issues with their gold filled (e.g., color fading, rusting over time)? Thank you for sharing your experience.