Dear Deb, In my fabrication classes I have used a glue stick for many
years. Here’s another tip. Make sure you pierce the design right
away. If you wait a day or two the glue will dry and the design come
off. Trying to realign the design with the piercing can be tough. If
the design does separate, take a little of the fire coat alcohol
(denatured alcohol) and wet it. Let it dry. The glue will reattach.