On the Moh scale where does glass fall in hardness?
Thanks.
Carla
On the Moh scale where does glass fall in hardness?
Thanks.
Carla
On the Moh scale where does glass fall in hardness?
Window Glass rates a 5 on the Mohs Hardness Scale.
http://mineral.galleries.com/minerals/hardness.htm
Kindest,
David Wooley
Fredericton, NB
About 5.5 – see for a simple scale:
http://www.gwydir.demon.co.uk/jo/minerals/hardness.htm
jesse