Thanks to Stanly Bright and a buddy of mine Kenneth Johnson for
giving me some inspiration and knowledge base for trying this…

Right now im still tweaking details but did a small write up on how
I was able to set a hand full of 4mm faceted stones into stainless
steel plate with vairous degrees of sucess.

www.patpruitt.com/study stone setting in ss>flush setting

Setting into complex surface will be a bit harder im sure, havent
tried it yet…anyhoo, let me know what you think of this technique
and any tips that you might have.

Thanks,
P@
www.patpruitt.com

www.patpruitt.com/study stone setting in ss>flush setting 

hello Pat, I can’t get this url to open. I tried via your website,
too, but can’t find this anywhere on the site. I would be interested
to read this, so any suggestions would be appreciated,

thanks,
Christine in S.A.
ps- your work is quite wonderful :slight_smile:

hello Pat, I can’t get this url to open. I tried via your website,
too, but can’t find this anywhere on the site. I would be interested
to read this, so any suggestions would be appreciated,

http://tinyurl.com/yn29lw

Direct link, I do not have this section linked from my home page.
You might have to copy and paste.

P@
www.patpruitt.com