Hi! I keep on warping cross lock tweezers, I think my flame may be too hot. Is there any way to bring the tweezer ends back together again?

Simply bend them back with pliers. That is going to happen from time to
time. If they close too hard and you want them softer you can heat them
more toward the hinge and them cool them quick and keep doing that till
they are how you want.
Shannon

Bend them back with pliers and have a few extras on hand with different sized and shaped ends.

Fantastic! Thank you both! :smiley: