Does fine silver wire come in anyhting harder than dead soft. I can
only find that form Rio. If not, how can I harden it?

Rudy, You could ask Hagstoz. They sell half-hard wire in 26 gauge,
and may have other sizes. Just don’t expect to get it quickly.

Janet

If you want to harden the wire get it a size or two heavier and draw
it down to size, that’ll do it! Jerry in Kodiak