To remove diamonds from old mountings, a cut-off disk mounted in your
flex-shaft can be used to cut-off the old beads, channel, or prongs.
CAUTION: Do not use this procedure on colored stones. They can be
damaged by the cut-off disk.

Brad Simon CMBJ
www.BWSimon.com

To remove diamonds from old mountings, a cut-off disk mounted in your
flex-shaft can be used to cut-off the old beads, channel, or prongs.

CAUTION: Do not use this procedure on colored stones. They can be
damaged by the cut-off disk.

But remember to keep your thumb nail on the stone, or it WILL fly
across the room, and you WILL not find it. experience talking here

ringdoc