When repairing hinges in bracelets such as tennis bracelets, often
the center knuckle is worn as well as the hinge pin. Build up the
hinge knuckle by fusing additional metal to it or attach a new one by
fusing the metal together, rather then soldering. Then when you
solder the new hinge pin in place, there is no solder on the inside
of the hinge that can flow and freeze the link. Brad Simon CMBJ