Hi al

I just started getting involved with selling Tungsten Carbide rings
and am curious as to how most online sellers are engraving their
rings.

Most laser engraving machines I’ve seen cost upwards of $20k+. I
know it is not feasible for most to buy these machines so how are so
many people offering tungsten engraving service for free or very low
costs? I’m just scratching my head here and feel like I missed
something! Thanks for any help.


#2

This is what we use in our shop.

http://www.ganoksin.com/gnkurl/ep81f2

I know, it’s almost six thousand dollars. I engrave tungsten all the
time. Tungsten doesn’t show up as bold as other metals and you
pretty much get one shot at it. If a mistake is made, that’s it.