I am a horologist in Cary, NC. I can make a pocketwatch dialplate
with feet in the correct positions and holes drilled. I am seeking
someone that can fire the dial with a thin perfect enamel coat. I
can then print. Anyone?

Thanks!!!
DennisK
ACRS
Cary, NC


#2

Hi Dennis,

I’ve been doing just that. I’m an Enamelist and I work in fine
silver or 18kgreen gold.

Send me an email off group at: Jenniferjh1 at mac dot com

Jennifer harris


#3

I’m an engraver who works with Anodized Niobium. I have given some
thought to engraving watch faces. Please let me know if you would be
interested.