I have just turned to cloisonne enamelling in the last year and so
far have made only endants and earrings. I am wanting to do rings and
link bracelets and I know other artists make them all the time but
the wearability seems in question to me–especially for link
bracelets. Are the rings and bracelets fairly durable or do the break
or chip easily?

J. Sue Ellington
http://www.jseenameljewelry.com

I think enamel on rings is an iffy idea. Do you want to enamel the
whole ring or just parts? Are you enameling on sterling or fine
silver. If the ring is thin, it can deform and pop enamels off.

marilyn