Back to Ganoksin | FAQ | Contact

[Enamel Bits] Ninomyia enamels

I am interested in the Ninomyia enamels. Would you give me some
on where I can purchase them and get some additional Thanks.

If in the U.S. you could try

Enamelwork Supply Co.,
Seattle WA
1-800-596-3257
Catalogue about $2.00 U.S., $4.oo elsewhere

David in Victoria

You can purchase them from:

Enamelwork Supply co.
Coral Shaffer
206-525-9271 for general questions.
1-800-595-3257 for ordering
1022 N.E. 68th St.
Seattle, WA  98115

Linda Crawford
Linda Crawford Designs
Willits, CA
http://www.lindacrawforddesigns.com

Ninomiya Enamels can be purchased from Enamel Works Supply in
Seattle, Washington. I believe that they have an 800 number. The
enamels fire very well and there is a terrific range of colors which
make shading a joy, however be prepared to do alot of washing, or
better yet get a set of graded sifters because there a a TON of fines
in these enamels. That aside, I have been using these enamels for
several years and am very happy with the results.