I recall a posting where someone listed the ingredients to make
electrocleaner similar to that sold by Rio. I believe it contained
Sodium Carbonate (washing soda), Sodium Hydroxide (lye), Trisodium
Phosphate (TSP), and Sodium Silicate (whatever that is).

Is anyone aware of the proper ratios of each, and is there any thing
that can be added or deleted?

I use the product to clean silver and find the water “sheets” off
after cleaning, very effective.

Thanks for all your help,
Jon

I recall a posting where someone listed the ingredients to make
electrocleaner similar to that sold by Rio. I believe it contained
Sodium Carbonate (washing soda), Sodium Hydroxide (lye), Trisodium
Phosphate (TSP), and Sodium Silicate (whatever that is). 

Here is a link to my article at the Ganoksin Project that addresses
this: http://www.ganoksin.com/borisat/nenam/cleaning.htm

best
Charles

sodium silicate is Water Glass, available at most pharmacies, or
they can order it from their simples supplier…simples is another
term for the single icompouinds like, flowers of sulphur,rose water
and glycerine,spirits of camphor etc…RER