I apologize for taking so long to get through all of my mail.
I’m under 600 messages in there now, and they are getting
older…

I’ve used an “industrial” sharpie for that purpose. It takes a
lot of abuse. I can usually get all the way through a cutting
project with marks left. It’s a fine point and has "industrial"
on the pen barrel.

Susan Embler