To all you Orchid folks out there that can read this reply,

Try Grobet File Company (William Dixon Co.) in Carlstadt, NJ (800)
847-4188

or

Otto Frei & Borel Co. in Oakland, CA (510) 832-0355 and ask for Steve
or John Frei

who will be more than happy to help you.

Sincerely, Richard Lucas Lucas Dental Company (718) 789-2604
http://community.webtv.net/lucadent


#2

Bad experience with Rio Grande, do not buy any findings there. I
bought a sterling silver mans ring finding terrible! Wall thickness
0.4mm Low end junk for $12.88 (production cost of the piece in mass
production approx. $3.05 very high calculated), could not be used.
When people start to save on silver thickness, then you know they are
a no good company. The problem is either greed or incompetence, both
are unacceptable. Rio Grande, I call them Rio Cheapo! Cheers, Klaus