dave… I also would be interested in diamond rifle files…
I live in Northern NJ…any chance of a store near me… thanks
calgang
dave… I also would be interested in diamond rifle files…
I live in Northern NJ…any chance of a store near me… thanks
Micro-mark is in Berkeley Hieghts NJ, But they only do mail order,
So I don’t think there’s much chance of browsing. I haven’t
tried recently, but about 2 years ago a friend and I called them
and asked if we could visit and they said “No”. OR maybe they justy
didn’t like the way I sounded?
T Goodwin
American Science & Surplus web page http://www.sciplus.com has
diamond files and diamond bits check under fix & build. This is a
trippy catalog everything from trash to treasure. I have ordered
tools from them and they are pretty good. Anna Martin
Dear Tim, some one else also gave me the micro mark phone number
and said to try so shall let you know… calgang thanks for the
help…
Hi…they also have those Tagua Nuts the “vegetable ivory” we talked
about on this site.
Sorry I’m late with a response, folks! Been on vacation! ![]()
A set of five diamond needle files advertised for $16.80; 8 piece
riffler file set (not diamond) for $6.95. Probably has diamond
riffler files, as well.
W.T. (or Wholesale Tool, not Western Tool as I previously stated),
where I’ve bought a lot inexpensive tools. They have seven
locations in the U.S.:
Warren MI: 800-521-3420; email WTMICH@AOL.COM
Indianapolis, IN: 800-551-2251; email WTIND@AOL.COM
Stoughton, MA: 800-343-1008; email WTMASS@AOL.COM
Charlotte, NC: 800-438-3580; email WTSOUTH@AOL.COM
Tulsa, OK: 800-331-4075; email: WTOKLA@AOL.COM
Tampa. FL: 800-237-4689; email: WTFLA@AOL.COM
Houston; TX: 800-231-4585; email: WTTEXAS@AOL.COM
If anyone wants more specific info (i.e., address, local phone
number) email me and I’ll provide.
Have fun,
Dave
Dave Sebaste
Sebaste Studio
Charlotte, NC (USA)
dave@sebaste.com
http://www.sebaste.com
Thanks dave for that source, meanwhile yesterday I recieved a
Micro-Mark Catalog, { <www.micromark.com>, 1.800.225.1066
}. They have a 5pc set for $12.95. #81414 pg 62. Micro-Mark is
primaily a model builder company, but they have much in small tools
and even some non-precious metal shapes and more… Thanks to all
responders, new to Orchid, efw