Back to Ganoksin | FAQ | Contact

Dessiccant and Silver tarnish

For any of you who, like me, are constantly struggling with your
silver jewelry tarnishing:

Apparently humidity has an effect at the rate silver tarnishes (lucky
me, leaving near the beach!). Anyway, a company called “Desiccare,
INC” out of Richland, Mississippi sells different sizes of pouches
filled with desiccant, which can be heated in an oven and then
re-used. Telephone (888) 932-0405 for more info.