hello, i am having trouble getting a beautiful frosted silver finish,
when i depletion gild my jewelry. any is greatly
appreciated. thanks in advance . shan


#2
hello, i am having trouble getting a beautiful frosted silver finish,
when i depletion gild my jewelry.  any is greatly
appreciated.  thanks in advance . shan 

Quench in pickle (be careful of splashes) from about 500 degC several
times. Burnish after every 3.

Cheers