Back to Ganoksin | FAQ | Contact

Cupric Nitrate as etching mordant

What is the formula for mixing Cupric Nitrate granules with water for electrolytic etching on silver?

According to Ben Dory in this article he wrote for SNAG, it’s 1 part cupric nitrate to 4 parts water, by weight.

Thank you so much! A very thorough article!

No problem, hope it works for you.