I have incorporated ashes into glass cabochons. I discuss the life
of the deceased person with the customer & then create an appropriate
image, for example a Yorkshire Rose. The ashes leave a light trail &
you would not know they were there unless you knew where to look.

Thank you for Orchid, it’s an education in itself.