We have come across an exceptional find. A solid copper cathode.
This is the raw copper as it is electrolytically grown at the source.
Out west here we see flat bed trucks loaded with these headed to the
mills. Sheet and wire would be directly wrought from this slab. It
weighs 196 pounds is 34 1/2" wide by 47 1/2" long it averages 3/8"
thick although the edges have a rounded effect and are about 1/2"
thick. Current bulk copper prices put it between $4 and $5+ per
pound. Tired of limitations, like to stretch raise? This may be a
once in a life time opportunity.