Closing up shop - selling materials and tools

I’m closing up my jewelry workshop and selling off my tools and materials. As several members of this forum recommended, I’m going to offer them to members of this forum first and then sell whatever is left on other marketplaces. This is a list of the materials that are available… I’ve included some photos but let me know if you need anything specific of if you have any questions. Let me know what you want and send me your email and shipping info. I’ll send you my contact and Venmo info. All payments must be made via Venmo. All shipping is via USPS Priority Small Box. If you buy multiple items I will try to fit it all in one box and let you know what the actual shipping cost is. Thank you for reviewing this post!

Granulation Spheres

I love granulated jewelry but making consistent spheres is challenging and buying them from the main supplier was prohibitively expensive. I convinced a precision semiconductor industry supplier to make some balls in bulk for me and I am selling the spheres I have left at very attractive prices. Here’s the details:

22K Yellow Gold Spheres - $400/dwt plus shipping and insurance

These are available in two diameters - .032” and .024”. Guaranteed uniform to within .001”. Minimum order 1 dwt. Shipping is $15 (in continental US only) and insurance is $10/dwt.

.032” size - 306 spheres/dwt

.024” size - 724 spheres/dwt

Fine Silver Spheres - $350/ozt or $225/half ozt or $150/quarter ozt (per size) plus shipping and insurance

These are available in three diameters - .028”, .024” and .032”. Guaranteed uniform to within .001”. Minimum order 1 ozt (combined). Shipping is $15 (in continental US only) and insurance is $10/ozt.
.032” size – 10,526 spheres/ozt

.028” size – 15,625 spheres/ozt

.024” size – 25,000 spheres/ozt

Fine Silver Fabricated Metal

All of these fine silver products are available at $75/ozt plus shipping and insurance. Each item can be sold separately but items cannot be split up. Most items were purchased from Hoover & Strong or Hauser & Miller.

Fine Silver Bullion – one 10 ozt bar available for $700 plus shipping and insurance

Hoover & Strong Casting Alloy These alloys are complete – you add only gold to get the desired karat. Refer to Hoover & Strong’s web page or catalog for details. Will only ship the full amount of each alloy. Shipping is $15 for whatever you order. The prices shown are 25% less than H&S’s prices

2 ozt YCB 10, 14 Yellow Alloy $60 (total for all 2 ozt)

1 ozt YCA 18 Yellow Alloy $27

1 ozt YRB 14 Royal Yellow Alloy $40

1 ozt P14 14 Pink Alloy $10

3 Likes

Update…

The 16g and 20g fine silver round wire is gone

All the fine silver sheet is gone

The YCA 18k alloy is gone

If you are interested in the granulation spheres, email me at mayflower@myhsh.net

1 Like

HI Ellen, Will you be listing any burrs or hand tools on this forum…?

1 Like

I will be listing some hand tools once the materials are whittled down. Too much to do it all at once.

1 Like