Clip earring findings

Good morning all, since I got such great answers to my pitch bowl
questions I think I will pose another question. I have not been
successful finding earrings findings for non pierced ears. I’ve
ordered from the usual suppliers and the clips have been very
flimsy. With very little pressure they seem to spring their little
levers and not stay tight. Is there a particular style of supplier
that has sturdy sterling silver clips?

Jean Menden

Clops are always a bit of a problem. The limit the size of the
earring. I like the clips I have bought from Rio Grande. Clips and
pin catches are the only items I tend to buy not made of sterling.
They are too soft when soldered. I like the clips with small rubber
pads. The people who buy those earrings seem to prefer them.