Back to Ganoksin | FAQ | Contact

Chicago pnumantic hammer

I just wanted to know how many of you guys use a Chicago pnumantic
hammer, and if you would reccomend one.

Scott
Berry’s Jewelry Co.
Nashville, TN
Cad/Cam & Laser services

I use mine daily. I would NEVER go back to a flexshaft driven
hammer. The Chicago pnuematic can be toned down to set the most
fragile stones or cranked up to hammer very thick metal. The biggest
advantage is the stroke speed. When you hammer gold down (or any
precious metal), it stays put and doesn’t bounce back. It’s a little
pricey, but once you use one, you’ll never look back. Ken