If you go to ebay.com and search for “centrifugal”, you will turn up
half a dozen centrifugal casting machines, all being sold by the same
fellow. I sent him an email asking what company made the machines,
and he replied Lucas Dental. I tried to find that company on the
Internet, but could not find it. The person selling the machines says
that he will sell them for $305, delivered to your door in the U.S.
(lower 48 states only). Is anyone familiar with these machines? Are
they worth the price?

Al Bayless

The answer to Mr. Al Bayless’ question (are they worth the price?)
definitely “Yes”

At $305.00 delivered (lower 48 states) where can you beat that
price?? and they are manufactured in the U.S.A.

The flask size capacity: up to 3-1/2" x 5" long.

The company “Lucas Dental” has been in business since “1930” and
there casting machine #750 “Giant” can be seen in the Rio Grande
catalog.

To further inquire about there machines, you can E-Mail them at:
LucaDent@Webtv.Net and mention that you heard about them on (Orchid)

Sincerely, Dick…

Mr. Al Bayless,

and the (Orchid) community and anyone else that may see this reply.

Lucas Dental Co. is a manufacturer of Centrifugal Casting Machines
and we have been manufacturing these machines since 1930, and I feel
that my machines are second to none in quality & design and $$ price.

To see a picture of our machines, please go to:
http://community.webtv.net/lucadent

If anyone should have any questions pertaining to any of my casting
machines, please feel free to E-Mail me, and mention that you heard
about my Company from (Orchid) and I will be more than happy to
answer all of your questions.

Thank you very much, Sincerely, Richard Lucas, V.P.