I’m trying to find someone who knows what Brazil Silver is. A friend
has what appears to be quite old cutlery with the following stamped
on the back, “Royal Manufacturing Co. Solid Brazil Silver” with a
crown on top. I won’t buy it (for melt down) without confirmation
that it is true silver. It in fact looks like nickle or German
Silver. I hope someone can shed some light on this, thank you in
advance,

John Barton


#2
I'm trying to find someone who knows what Brazil Silver is.

Brazil Silver is silver plate. A web search of “antiques, Brazil
silver” will get you started on the research.

^…^<
Susan Maxon