Back to Ganoksin | FAQ | Contact

[BenchTube] Gypsy Setting-Finish


#1

Now showing at the BenchTube

Gypsy Setting-Finish
Runtime: 5m 14s

In this second of two videos just on Gypsy Setting, I demonstrate
Bright-cutting inside of the “Gypsy” circle of metal. With this
final clean-up, I use my Flat-Faced, #180 grit Pumice wheel. It is
in contact all along the surface of the dome-shaped ring. No flat
surfaces are allowed, There are two axis’s of curvature & each must
be returned as originally made! There must be no contact with the
pumice wheel to the actual stone, lest the facets be totally ruined!
This can happen on many an occasion.

Watch Video: