950 TruPd solitair
Runtime: 2m 21s

This mount was fabricated using 950TruPd. Note that the raised areas
cause from hammering the taper in the shank were melted back into the
shank. There was little problem changing the width at the top and
adding it to the bottom. Build up areas are pit free using fast
building continuous TIG process.