Hello All,
I remember using asbestos back in 1973-76, when I was a student at the
Philadelphia College of Art (now University of the Arts, ah, progress),
while in the metalsmithing studio under Olaf Skoogfors and Leon Lugassy.
We had bags full of the stuff, and it was such a wonderful item to use!
I’ve never found anything with the same wonderful consistancy.