Back to Ganoksin | FAQ | Contact

April 2018 Schedule






Upcoming Events

1

Jewelry Class DC

Come see us at
1502 Massacheusetts Avenue
Washington, DC
Saturday, April 7th, 2018
9am-4pm
For more info please go to:

www.jewlelryclassdc.com

2

Guilded Lynx

Come see us at

458 Main Street

Ridgefield, CT

Thursday, April 12, 2018

10am-4pm

For more info please go to

www.guildedyynx.com

3

Hudson Valley Silverworks

Come see us at

77 Cornell Street

Kingston, NY

Friday, April 13, 2018

For more info please go to

www.hvsilverworks.com

Dave ,
Thanks for making the effort to travel up to Hudson Valley Silverworks.
I emjoyed getting home and reviewing the stones I bought .
Labradorite in particular is a favorite of mine.
The deep blue with very little visible cleavage is great.
Thanks again ,
Mike B.