Acetylene torch

I only worked in a shop which used natural gas; I have never “tooled
up” for natural gas I don’t have specifics. I believe manufacturers
provide different orifices for different fuel gases. Even if there is
some minor conversion expense natural gas is a great way to do
jewelry work if you have access.

Jim Small
Small Wonders