As I continue my research into buying a pulse arc welder, I have also looked at Argentium vs 925 Sterling. From what I read, I think that Argentium is not as heat conductive as 925 Sterling. That being the case, is Argentium easier to weld using a pulse arc welder than 925 Sterling? Thanks…Rob

I have an orio n 150 s2 and it weld Sterling fine. There is a learning curve though. What was a big help was going to a trade show were an Orion tech was there with the welders. I brought some Sterling parts and he helped me with the settings. It was difficult getting used to the microscope, so I purchased a screen that goes dark when I weld. This improved the flexibility. Vince Larochelle.